| Product |
Suitable For |
Temperature Range |
C.E. |
Addition Rate % |
Recommended For |
| MAGNASEED - 14 |
Grey Iron |
1350-1400 oC |
3.9-4.2 |
0.2+/-0.05 |
Chill reduction, improvement in machinability |
| MAGNASEED - 151/151M |
Grey Iron |
1350-1420 oC |
3.8-4.0 |
0.2+/-0.05 |
Chill reduction, improvement in microstructure & machinability |
| MAGNASEED - 156/156M |
Grey Iron |
1380-1430 oC |
3.7-4.0 |
0.2+/-0.05 |
Reduced end chilling, coupled with good quality microstructure & machinability |
| MAGNASEED - 16/16M |
Grey Iron |
1400-1450 oC |
3.7-3.9 |
0.2+/-0.05 |
Suitable for high grade cast iron having stringent microstructure. It increases tensile strength of the iron |
| MAGNASEED - 20/20M |
Grey Iron |
1380-1450 oC |
3.8-4.0 |
0.2+/-0.05 |
Improvement in microstructure machinability and also promotes pearlitic matrix. |
| MAGNASEED - IS |
S. G. Iron |
1400-1450 oC |
-- |
0.3 - 0.5 |
Used as post innoculant for improving nodularity and nodule count. |